Does anywhere in AWS D1.1 says for percentage of NDT to be carried out either in fabrication or in field welds.
--


Regards

Biinoy L

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKrfo%2BBUL%2BRvbyTa%2BLgDO3MV%2BahkW8JibkGStv6r4grX%3Dd9D6g%40mail.gmail.com.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...