Tuesday, March 31, 2020

Re: [MW:30678] Production test coupon

Kindly check UCS-66 for impact exemption in ASME SECTION VIII DIV.1
Product-SA 516 pressure vessel 

Ihsan Kareem Anjum
API Inspector
API 653, API 510 and 570
ASNT LEVEL ll
+92-3346985641
+92-3036593031


On Tue, Mar 31, 2020 at 8:26 AM 'GENE MATSKO' via Materials & Welding <materials-welding@googlegroups.com> wrote:
                                                                                                    
  
ASME SECTION VIII DIV.1
Product-SA 516 pressure vessel
Field Test Coupon Procedure:
 Simply take test coupons onto scaffold near the actual field weld. The test coupons must be of the same material and type etc and backed up with documentation. Set up test coupon in same position as actual field weld.This was the way we done production
test coupons in the past for ASME-Section VIII, DIV I when required. 
I hope this helps                                                                               
Gene Matsko


On Monday, March 30, 2020, 12:50:30 AM CDT, Sachin Dhiman <sachin.dhimanet@gmail.com> wrote:


In relation to ASME SECTION VIII DIV.1
Product-SA 516 pressure vessel


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/675cdfd0-2112-4f3a-afcc-95aa94dcdf47%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/630815146.1507293.1585608967811%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxpTBwn7KgX%2BhTbR%3D%2BM_N3zdgpF6bkLp0WGSffCco6iXYgXRQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...