PQR and WPS are different.
WPS is procedure for performing the welding on jos. PQR is like performance test to check if this welding is possible. 
Rgds
Prakash Gotimukul
Consultant ASME/ISO/PED/IBR
Mob:+971 55 711 4761


On Sat, Mar 21, 2020 at 12:04 AM Venkat Ramana <venkatgps.ramana@gmail.com> wrote:
Dear Experts,

My query is that, is there any mandatory by TPI approval (Seal and Sign) on every WPS ?? even though they have already sign into the supporting PQR'S....

KINDLY CLARIFY WITH RELEVANT CODES AND STANDARDS.


Thanks & Regards

Venkat
+91 9676061257

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsPJvRAQu5%3DeNN0L8qFX_-SjVMCK-YAkoQ2AjshHsBmPdw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4qLycxoBV%2BH-t1bvVr6xtmaJvES7G52Cf79kuqS1JeQFWQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...