Re: [MW:30578] Glass bead blasting technique

Sir pl share the specification or reference standard

On Tue, Mar 3, 2020, 10:37 Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Yes

On Mon, 2 Mar 2020 12:32 pm Hrushikesh Sangamnerkar, <hrushi612@gmail.com> wrote:
Dear experts,

One of our suppliers proposed to carry out Glass Bead Blasting on SS 347 ID surface.

Is there any ASTM specifications and standard and is this method acceptable?

Pl share your views.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2rUpUd-3L4E-1g5XOwRDS2fOoC2mY%3DD2ZFeczbt77zaRw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eND-J8SuUXkTiQCpCHGmaGrk4yNtBjTxovwcRvWh%3D3R8Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2oO-jeKeda9qi_XStbkUFQ5HGp42d%3DzpWmqdkAtqPUgqw%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...