Friday, March 6, 2020

Re: [MW:30607] Opening of Nozzle in Weld in Dished End.



Generally client will restrict any openings in pressure retaining welds, however code requires additional RT 

Thanks and Regards

Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Fri, Mar 6, 2020 at 10:44 AM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Dears
         Construction Code-ASME Sec 8, Div-1.   Nozzle hole is fouling in the  Welding of Dished End Petal Construction. Is it permissible?. Throw your valuable inputs. 
 
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePwMfsfsPEWEwe8beOO8NQVY-8EPrkxMc%3DF_jFFKnV6hA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaSVcEgHgS2pLCpFaZ21bC0-LWERWFMpRZjCXQg4TJt_kz%3DKA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...