TPI not a ASME Code requirement.
But it depends on Client Specification and Client Acceptance. Generally it is a practice to Qualify Welders & PQR's with reputed TPI so that it can be Accepted by all Clients.
Thanks & Regards
J.Gerald Jayakumar
On Tuesday, March 24, 2020, 11:33:24 AM GMT+7, NARK <nidhin595@gmail.com> wrote:
Dear,
The TPI is not mandatory for the welder qualifications and welding procedure qualifications as per the code,if the client specification or contract is mentioned any requirement ,then it become a mandatory requirement...
Regards
Nidhin r k
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/b9fe3e02-6868-47e3-bc35-29d142041fe1%40googlegroups.comhttps://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
.
Comments