[MW:30580] Patch Plate Thickness - API 650 Tank

Dear Experts,

Construction Code: API 650
Annular PlateThickness: 13.5mm
Bottom plate thickness:8.0mm
       We are in a position to weld "Patch Plate" on the Annular ring plates.All the repairs are not in the critical zone (3"inch as per API 653). As per API 653 the patch plate thickness within the critical zone is  1/4" maximum. Could you please suggest the thickness requirement for the "Patch Plate" beyond the critical zone and within the annular ring plate.

Please kindly give your inputs with code reference.

With Regards,
N.S

With Regards,
N.Shanmugam


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaJw0JR6FkAWJ8fgsj7W-vi7VHEUoD%3DoWq3PhEVhh9itp0muA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...