max 1.35 is acceptable
btw did u succeed in flattening test?


On Mon, 4 Nov 2019 at 16:44, Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:
Dear all,

We have LTCS Pipe(18" 160 sch A333 GR. 6), completed the flattening test. In the chemical analysis report shows manganese composition value is 1.49 but the range is between  . 290 to 1.06

Shall we accept dis. Experts share your opinions


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubm9HiXnABD8fG%3D%2B3LJHPEOJ_PGR%3DVaCwALuEzQqHV5iwg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...