[MW:30213] Specific acceptance Radiography Criteria for Aluminum Welds

Dear Experts,

What is the acceptance criteria for porosities in Aluminum welds subjected to Radiography Examination?

I am having only 3 porosities scattered (1.2mm dia.max) in the entire weld length of 350mm coupon.

Coupon thk = 4mm
Welding process - GTAW

Require your valuable inputs.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2q_sMYR5rPWJLW497pNN7XkUPs7R2grHAxkZG87fgHhHA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...