Re: [MW:30193] Alternative for flattening test of LTCS pipe

 Dear raghuram, 

    Are you asking the material standard of the pipe it is A333 Gr 6

On Fri, 1 Nov, 2019, 4:34 AM Raghuram Bathula, <raghurambathula@gmail.com> wrote:
what is your product standard? 

On Fri, 1 Nov 2019 at 08:54, Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:
Dear All,

We are facing one problem for Flattering test of one LTCS Pipe.


 For Pipe Size 18" x Sch.160 (45.24 mm Thk) – Flattening test result not satisfactory because UTS machine capacity could not achieved the flattening height as per requirement. Obtained Flattening Height – 330 mm (Req. 286.44 mm)  

 

Kindly advice alternative for the following 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubnAUC-JidhwbzpQAwOn%2BJMuX-%3DbWHaN07evcSuBf2Sjgg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0z2k6j-Njf%3DgBPCpxF7MKK2mdrns78TKo8iAgLwsjb%3DQQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...