Hi

Any body has experience in field piping solution annealing . I like to get support  requirement  ( calculation or recommendations or any reference material) while doing the annealing  as the temperature is around 2100 F.

This is 26" 1.6" thick 347H material at service 650 degc .

This has simply supported and cantilever situation 





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABhoKTCH8XkqFpHYBS%3DPXmW3ooh6anqSNvNtcrMQNFefw%3D%3D5Uw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...