Monday, November 4, 2019

Re: [MW:30204] Manganese value is more

max 1.35 is acceptable
btw did u succeed in flattening test?


On Mon, 4 Nov 2019 at 16:44, Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:
Dear all,

We have LTCS Pipe(18" 160 sch A333 GR. 6), completed the flattening test. In the chemical analysis report shows manganese composition value is 1.49 but the range is between  . 290 to 1.06

Shall we accept dis. Experts share your opinions


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubm9HiXnABD8fG%3D%2B3LJHPEOJ_PGR%3DVaCwALuEzQqHV5iwg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...