Tuesday, November 5, 2019

[MW:30212] Hardness Test

Dear All,
Pl clarify, how to take hardness measurements on welds after PWHT for SA 516 Gr 70 material.
Is there any code reference?

Thanks& Regards,
Venkatramulu

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdHYCPSu_LL3RaVz%2B7Q10FSw8dED8kXGn_y9oWQyFoTs4A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...