You can use as reference AWS D1.1:

 

·         mild steel (yield strength up to 36 ksi [250 MPa])

·         medium-strength steel (yield strength between 36 ksi and 65 ksi [250 MPa and 450 MPa])

·         high-strength steel (yield strength between 65 ksi and 115 ksi [450 MPa and800 MPa])

 

 

De: PUB:'Mohamed ali' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Enviada em: domingo, 4 de dezembro de 2016 12:24
Para: materials-welding@googlegroups.com
Assunto: [MW:25792] High strength material and Low strength Material

 

Dear Experts, 

 

How to classify High strength material and Low strength material, because our client says SA 36 and S 275 JR are high strength material, we have to prove that both of the materials are Low strength material.

 

If Low strength material - 2.2 certification enough.

 

please ...

 


 
Thanks & Regards,
 
M A Samsudeen

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/365800098.6115272.1480861457939%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...