Dear Experts,
I have a Groove weld joint of thickness 40mm. The standard i need to follow is API 6D..
Welding procedures qualified under ASME sec.IX without PWHT with a test coupon of 50mm thickness of material ASTM A516 gr.70..
API 6D states " PWHT shall be performed in accordance with the applicable material specification or design code"
My material specification is ASTM A516 gr. 70 and Design code is ASME Sec.VIII Div. 1
A516 standard doesnt states welding or PWHT requirement, whereas ASME sec.VIII states - thickness above 38mm PWHT is mandatory..
Can i take the material specification to justify for not performing PWHT..
Please advise
With regards and thanks
Vadivel M

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d3a93cea-c615-43c9-9089-177d9cbcc77e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...