Friday, December 30, 2016

Re: [MW:25855] PWHT reqmt for welds as per API 6D

In no case. You have to comply with VIII-1



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Vadivel Mahadevan <vadivelmahadev@gmail.com>
Date: 30/12/2016 05:40 (GMT+02:00)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25854] PWHT reqmt for welds as per API 6D

Dear Experts,
I have a Groove weld joint of thickness 40mm. The standard i need to follow is API 6D..
Welding procedures qualified under ASME sec.IX without PWHT with a test coupon of 50mm thickness of material ASTM A516 gr.70..
API 6D states " PWHT shall be performed in accordance with the applicable material specification or design code"
My material specification is ASTM A516 gr. 70 and Design code is ASME Sec.VIII Div. 1
A516 standard doesnt states welding or PWHT requirement, whereas ASME sec.VIII states - thickness above 38mm PWHT is mandatory..
Can i take the material specification to justify for not performing PWHT..
Please advise
With regards and thanks
Vadivel M

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d3a93cea-c615-43c9-9089-177d9cbcc77e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...