[MW:25845] RE: 25843] Welder performance for Temper Bead Welding

Hi Karthikeyan,

 

The default rule is ASME Sec-IX, QW-290. If  the applications are for pipelines, then you need to follow the guidelines of Piping Research Council(PRCI) also as additional resource.

 

Where this technique would be applied, and what’s the grade of steel in question?

 

Appreciate your response.

 

Thanks.

 

 

 

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgoswami@quickclic.net

pradip.goswami@gmail.com

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Karthikeyan Muthuvel
Sent: Monday, December 26, 2016 7:02 AM
To: materials-welding@googlegroups.com
Subject: [MW:25843] Welder performance for Temper Bead Welding

 

Dear Experts,

 

Could you please clarify the mentioned subject, is it necessary to qualify the welders to perform the Temper Bead weld. If yes, what is the procedure/method for qualifying the welders.

 

Thank you,

Karthikeyan M

QA/QC Team 

Al-Muzain, Saudiarabia.

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL7K%3D_%2BqTaAvJofJjv7KraxBMufM0ZmpsLPTpQ2%2BRSqKrzkrtw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...