Re: [MW:25813] Temporary piping used in hydrotest - ASME B31.1

Thank you for sending.

Could you please inform for the reference for the table from code, standard.

Kind Regards.



2016-12-10 7:58 GMT+01:00 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com>:
Hello Zakaria,
Please see below
 
Best Regards,
Shashank C Vagal  (Quality Adviser)
Neo Metal-Analyst & NDT Services (Approved by IBR, Thermax, AERB)
Regd Office: 301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA
Tel: +91 22 2611 6640 / (+91) 9821386292 /  8082395502 / 9819191861    
Works Office: A-25, Geet Siddhee, Sector No. 11, Pradhikaran, Gat No. 62, Boradewasti, Moshi, Dist: Haveli, PCMC, Pune – 411044, Maharashtra, India   
www.neometalanalystndt.com / enquiry@neometalanalystndt.com / nach_sam@yahoo.com



From: Zakaria ghrab <zakaria.ghrab@gmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Saturday, 10 December 2016 8:10 AM
Subject: [MW:25809] Temporary piping used in hydrotest - ASME B31.1

Dear Experts,

  Could you advise us: For piping system hydrotests power plant project, we ave to prepare and use some temporary piping. The issue is :

- Is it Manadatory to perform NDE in related welds  and also PWhT
NO FOR EITHER, 
BUT FOR PWHT - ANY WELDING INDUCED STRESSES IN EXCESS OF YS MAY BE UNDESIRABLE.
PERFORMING NDE ON ALL INCLUDING TEMPORARY MEMBERS WILL BE IN YOUR BEST INTEREST. IF A JOINT LEAKS BECAUSE OF ANY WELD DEFECTS, YOU WILL FACE EXTRA COST, ADDED TIME, RE-SCHEDULING, ETC  DUE TO  RE-HYDRO.
- For Flange fabrication, how to use plate thickness, any code or standard reference !
PLEASE SEE ATTACHED


Please advise according your experience and with ASME reference .

Thank you.

--

Thanks and Regards, ?
-----
زكرياء غراب
GHRAB Zakaria 
Tunisia : +216 96 635 805

Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD8EeB15hqZTM7eP9EyGTUCdawvDKKHZxHHC%2BK5NhRbeOLt8YQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1461469163.207663.1481353081256%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.



--

Thanks and Regards, ?
-----
زكرياء غراب
GHRAB Zakaria 
Tunisia : +216 96 635 805


Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD8EeB0tGZC%2BpOOwgiEAttxTSe_gVzed0C469z1GjBqvDPRr5g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...