[MW:25828] Distortion controlling method while using ASTM A 588 grade steel.

Dear Experts,

We are working for a client with ASTM 588 grade B material which is atmospheric corrosion resisting steel.
With SMAW and ASW E 8018 W2 electrode.

We are facing distortion problems -  bend / tilt, while fabricating of I beam structures.

Even after giving adequate supports distortion happening. 
'
My question is is by heating the job and rectification is the only process OR cold pressed rolling is advisable for this material.

Please advice.

Thanks in advance,

Regards,

Dattu.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/215ee7db-4111-4a74-84f7-0bb2bfeb11f5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...