Re: [MW:25851] RE: 25843] Welder performance for Temper Bead Welding

You have to find the way through the labyrinth of QW-290 in ASME IX

2016-12-27 7:05 GMT+02:00 pgoswami <pgoswami@quickclic.net>:

Hi Karthikeyan,

 

The default rule is ASME Sec-IX, QW-290. If  the applications are for pipelines, then you need to follow the guidelines of Piping Research Council(PRCI) also as additional resource.

 

Where this technique would be applied, and what's the grade of steel in question?

 

Appreciate your response.

 

Thanks.

 

 

 

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgoswami@quickclic.net

pradip.goswami@gmail.com

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Karthikeyan Muthuvel
Sent: Monday, December 26, 2016 7:02 AM
To: materials-welding@googlegroups.com
Subject: [MW:25843] Welder performance for Temper Bead Welding

 

Dear Experts,

 

Could you please clarify the mentioned subject, is it necessary to qualify the welders to perform the Temper Bead weld. If yes, what is the procedure/method for qualifying the welders.

 

Thank you,

Karthikeyan M

QA/QC Team 

Al-Muzain, Saudiarabia.

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL7K%3D_%2BqTaAvJofJjv7KraxBMufM0ZmpsLPTpQ2%2BRSqKrzkrtw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!~!UENERkVCMDkAAQACAAAAAAAAAAAAAAAAABgAAAAAAAAA5rYMdESrHU2r7z2aNylU0sKAAAAQAAAAwO8LScbCWUq3VhJVHFdX5AEAAAAA%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40A3r%3D4Q1W_-ePEUmU2Wzx5vffQArEDYr%2Bc6gev9Qnf0Vg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...