Dear Prem,

I am only ASNT Level II and during Level II Certification same thing is explained to me as you suggested,
But L&T Level III and AI given instruction that any way they can Clean since no where it is specified to clean in Uni Direction as well as Time to Clean.
They Have Instructed clean the Penetrant until the any penetrant races visible.
Cleaning time They are taking 10 to Minutes.

Since I don't have any ref in Code and Specification or Any Std. ASTM E 165 so I can't argument.
If you have any ref. Pls tell me.

On Wednesday, October 12, 2016 at 1:01:00 PM UTC+4, israr wrote:

Dear all
During pt examination on weld we are using wire brush wrapped with cloth to remove penetrant from the grooves of weld passes.
Can anybody reply. Is it correct practice?
With ref to code and std.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/02f0e6ad-bcca-40e6-acbc-df2aef87e5dc%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...