[MW:25175] Re: RF pad clashing with circumferential pipe weld joints

Dear Jijil,

Take RT of the  circumferential joint and before  pad fit up flush the joint area  and if need DP to be carried out 

On Saturday, July 30, 2016 at 3:31:12 PM UTC+5:30, jijilalkm2 wrote:
Dear Experts,

Refer to subject line and attachment , An RF pad is coming closely  with the circumferential weld of a lateral Tee.

Please advice how to resolve it. Code is ASME B 31.1.



Best Regards,

JIJILAL K.M. 
Thai Jurong Engineering Ltd,
KCE SPP Project,Thailand


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ad06e36c-397f-474b-9c64-3c7440598829%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...