[MW:25294] Re: Welder qualification

Dear Krisanu Bhunia, 

Refer to clause no. QW-191.1.2.2 (b) (3) Qualification Test Welds of the ASME Sec IX - 2015 -- Assuming test coupon is greater than 3 mm.
You can get the acceptance criteria for cluster porosity.


Regards
MK




On Sunday, 21 August 2016 18:39:30 UTC+8, Krisanu Bhunia wrote:
Daer.ALL
Please tell me cluster porosity acceptance limit for Welder qualification test as per ASME XI or VII.

 Regards
krisanu bhunia

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4f4aa579-8022-40f6-9140-3415cf03d3f4%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...