[MW:25241] Regarding liner plate to chute plugs welding

Dear sir,

We are installing chute in material handling work.

My query is that,  liner plate to chute plug welding is allow or not?.

Generally, liner are replaceable, i.e. in bolting ( chute to liner).
So if we plug weld it, it not possible to replace easily.

So, plug welding allow, then where and why ? ( in terms of function).

Regards
Prasad rode
7064460053

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bk3Rc9oBq9zAqw5aMNMi4MWbcPo9wHm_Cn_GLjim-UPjoWeSw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...