Please change your ferrite meter readings to %ferrite. Your problem solved.


On Aug 23, 2016 08:27, "Mohammed Azharuddin" <humaidazhar@gmail.com> wrote:

Dear Experts,


We have performed qualification on Duplex stainless steel BM UNS 31803 welded to itself with filler ER2594. Shielding gas AR+2% nitrogen


Ferrite measurements of welds were carried out as per ASTM E562 and AWS A4.2.


Client has rejected these values as the correlation is not appropriate.See below reported values and client comment.


From client point of view ,It should have been like VOL % FRRITE = 70% FN VALUE.


Your valuable advise will help us to save this WPS from being rejected.


Many Thanks


Regards,

Mohammed Azharuddin

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEeeqaKkHHhBuUFxq5QX32g5vOV4JrYdb1X0fWAyf9qSrZHN0w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE4SttEeF_9n_4nE03Ur3E0osSTV6jrz5VMiqjJx-au_jbzf6A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...