Sunday, August 21, 2016

[MW:25275] Post Forming Heat Treatment of SS316L Dish

Dear All,

Code: ASME SEC VIII-1

Post forming Heat Treatment of Dish...

MOC: SS316L

Design Temp 85°C

Fibre Elongation: 3.6%

UHA-44 table does not show values of Fibre elongation..

Is PFHT required for this dish.

Kindly advise

Ahmed

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BL7tiPwcXf8BVFYiF_b%2BCF3jdfsjhVdQGAyK-FfvAhpWOZDOQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...