Monday, December 29, 2014

Re: [MW:22658] Corrosion & Painting

Hello Dear,
I think so you need to have HVOF high velocity oxygen fuel coating on those equipment's. It will be expensive but surely it can resist wear & tear done by sand. You can check more details. This is modern technique of painting may be the best one also.

Regards,
Addil Yusaf   

On 24 December 2014 at 15:18, Ali Al-Zawamri <alzawamri@gmail.com> wrote:
Dear,

We are facing a lot of corrosion and rusting in our plant.
Please give your advices on the following:-
  • Best surface preparation where sand plasting can not be done.
  • Best painting to be used in high humid areas and where surface preparation can not be done by sand plasting?
  • After repairs and painting, rusting will take place within one year.
Your input will be highly helpful.

Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Mechanical Engineer 
Daewoo Enginnering & Construction.
Patrind Hydro Power Project Pakistan.
Contact Number : 03448834732

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...