Monday, December 29, 2014

[MW:22661] Which welding electrode suitable for SMAW of ASTM 135 ERW pipe to pipe welding & ASTM 53 ERW pipe to pipe welding.

You can try with E6010 or E7018, what grades are you going to weld?

Sergio Muñoz
IWE-IIW
http://Weld-ING.blogspot.com

--