[MW:22615] Re: DPT for Structural welding

Dear Feroz; Dye Penetrant testing for structural welding, is not specified by any code. It may be done for the satisfaction of client or third party . Find DPT considerations in http://www.weldpedia.com/search/label/Dye%20Penetrant%20Examination

On Friday, April 1, 2011 4:35:07 PM UTC+5, Feroz Mohammed wrote:
Dear All
 
Can any body tell me if it is required to do DPT for root run & after final welding in structural steel. If yes how much percentage
 
CODE: AWS D1.1

--
Thanks & Regards
Feroz Mohammed
Deputy Manager-QA&I
LANCO Infratech Ltd.
È : +91 9650490097
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...