[MW:22572] RE: 22570] Lamination check pipe cutting by cuting tools.

With any method of cutting you could either cut through a lamination, or cut so that you have a lamination close to the bevel but not actually emerging on the bevel. Apart from UT  you may do MPI on the cut edge to see if a lamination is apparent on the end bevel. What you decide to do depends on whether the lamination check by either is required by the specification. If the final welded joint is subject to UT this will be revealed and you will have a cut-out.

 

AKD

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of S.Mohammed
Sent: 14 December 2014 15:22
To: materials-welding@googlegroups.com
Subject: [MW:22570] Lamination check pipe cutting by cuting tools.

 

Dear all,

API 8/10" pipe sch40.

Lamination cheking bevel edge require if pipe cut with pnematic cutting tool?

Or only require when flame cutting involve?

Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...