Re: [MW:22630] Positive Material identification (PMI)

Fill the system with water, wait for 1 day and dump flush, in case of CS root rusty water will come out (experienced in the past after hydrotest)

Regards

Jurgen Prinsen MSc IWE
----- Oorspronkelijk bericht -----
Van: "Zakaria ghrab" <zakaria.ghrab@gmail.com>
Aan: materials-welding@googlegroups.com
Verzonden: Dinsdag 23 december 2014 17:48:45
Onderwerp: [MW:22627] Positive Material identification (PMI)



Dear all,
 
  Could you please help us.
 
In our project, austenitic stainless steels welds, we have a doubt for some welds that may be welder used GTAW carbone steel filler metal in root pass.
 
We propose to use PMI inspection but we're not sure about result fiability (root CS + Cap/Filling SS).
 
Regards.




----- GHRAB Zakaria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
For more options, visit https://groups.google.com/d/optout .

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...