Dear GHRAB Zakaria
If you want to get the exact Testing proof has been done by using
copper sulphate solution apply over the welding area if color did not
change the exact ss filler is used if colour changing means filler
wire mixed try this test
Regards
Pravean
On Thu, Dec 25, 2014 at 11:27 AM, Asif Raza <asif.raza@yascotech.com> wrote:
> Do PMI test through spectro machine.
>
> Jon Rajan
> Welding Engineer
> KSA
>
> -----Original Message-----
> From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of J Prinsen
> Sent: Wednesday, December 24, 2014 1:41 PM
> To: materials-welding@googlegroups.com
> Subject: Re: [MW:22630] Positive Material identification (PMI)
>
>
> Fill the system with water, wait for 1 day and dump flush, in case of CS root rusty water will come out (experienced in the past after hydrotest)
>
> Regards
>
> Jurgen Prinsen MSc IWE
> ----- Oorspronkelijk bericht -----
> Van: "Zakaria ghrab" <zakaria.ghrab@gmail.com>
> Aan: materials-welding@googlegroups.com
> Verzonden: Dinsdag 23 december 2014 17:48:45
> Onderwerp: [MW:22627] Positive Material identification (PMI)
>
>
>
> Dear all,
>
> Could you please help us.
>
> In our project, austenitic stainless steels welds, we have a doubt for some welds that may be welder used GTAW carbone steel filler metal in root pass.
>
> We propose to use PMI inspection but we're not sure about result fiability (root CS + Cap/Filling SS).
>
> Regards.
>
>
>
>
> ----- GHRAB Zakaria
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
> For more options, visit https://groups.google.com/d/optout .
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
>
>
> -----
> No virus found in this message.
> Checked by AVG - www.avg.com
> Version: 2015.0.5577 / Virus Database: 4257/8802 - Release Date: 12/24/14
>
>
> -----
> No virus found in this message.
> Checked by AVG - www.avg.com
> Version: 2015.0.5577 / Virus Database: 4253/8784 - Release Date: 12/22/14
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...