Re: [MW:21304] Use of Filler Wire E71T-1C for vessel with MDMT -29°C

No Prohibition for use of FCAW from code.
But many client specification prohibit use of FCAW on Pressure Vessels.


On Tue, Jul 1, 2014 at 7:00 AM, Mhaskar Aly <mhaskar.aly@gmail.com> wrote:

Dear Friends,

 

We have

·         FCAW filler wire E71T-1C (Impact tested @ -20°C as per MTC)

·         Vessel (SA516 Gr 70; MDMT -29°C; Impact test exempted)

 

Can we use this filler wire for welding on above vessel for:

1.       Nozzle to Shell weld

2.       RF Pad to Shell weld

3.       Vessel external Attachments with pad.\

4.       Saddle Pad to Shell weld

 

Kindly provide Code Reference

 

Thanks & regards

 

Ali Mhaskar,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...