Re: [MW:21422] Underwater Welding_Grade 4.6 Bolt on to Grade 250 plate.

What are the carbon equivalents of the plate and bolts?!?

Regards

Sayee

On Thursday, 10 July 2014, Pottayil, Biju <Biju.Pottayil@leicon.com.au> wrote:

Hi Gents,

 

I would like to request your valuable opinion/time regarding 6mm Multipass fillet under water confirming to AWS D3.6-2010 acceptance to Class B (fit for purpose). Materials to be used is AS1111 Grade 4.6 Bolt over AS3678 Grade 250 26mm plate. This is required for repair/replace by welding the anode brackets in place, so no special requirements need to be considered.

 

Could you please advise, whether there is any major risk in doing so.

 

I understand the weldability of the 4.6 grade bolt is not that excellent and will have issues related to HICC. We are using the consumable Hydroweld FS as per attached. As this weld is not that for a critical application, please provide me your expert advice.

 

Please view below the pWPS extract I prepared FYI.

 

 

 

Procedure:

Grind off the stud back to the doubler plate, including any paint unit clean shiny steel surface is achieved.

Weld a M20 Grade 4.6 Hex Bolt to the doubler plate with CFW  all around.

Reinstall the anode bracket to this M20 Stud.

 

 

 

 

 

 

 

 

Regards,

 

Biju Kurian Pottayil


*****************************************************************************
This email, and any files transmitted with it, are confidential and intended for use by the addressee only. The confidential nature of the information contained in the email and/or file attachment is not waived, lost or destroyed if it is sent to other than the addressee. Use or dissemination of the information contained in the email and/or file attachment, by a recipient other than the addressee, may cause commercial damage to both/either the sender and/or addressee. If you are not the addressee of this email/file attachment contact the sender immediately and delete this email/file attachment.

All email communications to and from this company are filtered and stored for risk management purposes in accordance with our Computer and Email Policies. Please contact our Privacy Manager on +612 8668 6947 if you would like further information about our Policies in regard to these issues.

*****************************************************************************

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...