Skip to main content

RE: [MW:21436] welding ss pipes with R316LT1

Hi Deepak,

 

There is no way you can avoid slag going to otherside-in fact purpose of a flux-cored TIG filler  is to produce fluid slag acting deemed purging.

 

I would suggest you may look at the attached PDS of Avesta 316L/SKR -4D electrodes recommended for such applications.

Hope this helps..

Thanks

 

With Regards

Amitabha Bhattacharya

Head - Application Technology

 

voestalpine Bohler Welding India Pvt. Ltd.

voestalpine Bohler Application Technology Centre

A-140, Metropolitan, ground floor

Road no. 23, Wagle Industrial Estate

Thane – 400604, India

T. +91-22-2582 8855

F. +91-22-2857 4445

M. +91-98 33998246

amitabha.bhattacharya@voestalpine.com

www.voestalpine.com/welding

voestalpine – One step ahead

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of DEEPAK cb
Sent: Monday, July 21, 2014 2:18 PM
To: materials-welding@googlegroups.com
Subject: [MW:21434] welding ss pipes with R316LT1

 

Dear All

 

I need to do some repair works in 316L pipes. So purging in these pipes are a problem and so am planning to use R316LT1-5 from the manufacture kobelco. Welding process is TIG. As per the manufacture R316LT1 does not requires any purging and can do the root run using the filler wire. But slag will be formed in the back side of the root. IS there any way to remove these  slags as it is drinking water line.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...