Dear Mohd,
For detail information, 
 what is the quenching temperature of the SS316L material and is the any proper record of the welded joints temperature a second before water shower ing on the joints. ?


Sent from Samsung Mobile



-------- Original message --------
From: Kannayeram Gnanapandithan <kgpandithan@gmail.com>
Date: 23/07/2014 12:41 PM (GMT+08:00)
To: materials-welding <materials-welding@googlegroups.com>
Subject: Re: [MW:21445] SS welding quenched by water


Boxbe This message is eligible for Automatic Cleanup! (kgpandithan@gmail.com) Add cleanup rule | More info
no

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY


On Wed, Jul 23, 2014 at 2:01 AM, S.Mohammed <mohd52100@gmail.com> wrote:

Dear all,

316L welding joints(6joints) were hot  welding condition quenched by cold water (20C) due to leakage...on upper side pipe.

Is there is metallurgy effect on SS welding due to this sudden quanching??

Regards
Mohd.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...