Re: [MW:21427] RESULT-CSWIP-3.1

Dear zubair,
 
To certify 3.0 who also have to do fillet weld practicals.as it is not included in 3.1.so they do not certify 3.1.
 
 
Regards,
 
prashun
 


On Sun, Jul 20, 2014 at 9:09 AM, zubair <zubair.me@gmail.com> wrote:
Dear all

In the reference to the above subject i would like to ask you ,I have cleared Four paper-in CSWIP 3.1 EXAM
  1. PRACTICAL BUTT WELDED BUTT JOINT IN PLATE  - PASS
  2. PRACTICAL BUTT WELDED BUTT JOINT IN PIPE     -PASS
  3. PRACTICAL ASSESSMENT OF 2 MACROS                -PASS
  4. GENERAL THEORY                                                      -PASS
  5. but unfortunately failed in Technology theory paper  in  CSWIP 3.1 Exam & Retest Also failed.

As per TWI for CSWIP 3.0 to required to have clear that paper- PRACTICAL BUTT WELDED BUTT JOINT IN PLATE & PRACTICAL BUTT WELDED BUTT JOINT IN PIPE, for the certification, that one already cleared as per my mark sheet.

My Question is , if i am eligible for CSWIP 3.0 CERTIFICATION from the TWI because i have passed that paper as said above.

Why they are not certified CSWIP 3.0

Thanking for your reply in advance

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...