Dear Sir
As reference you can use the code AWS B2.4-2012.
Greetings,
Met. Eng. WZA
> Subject: [MW:21437] WPS details for HDPE
> From: mohdfirdaus.abdrahim77@gmail.com
> Date: Mon, 21 Jul 2014 22:48:23 +0800
> To: materials-welding@googlegroups.com
>
> Dear all,
>
> Can anybody guide me for preparation HDPE WPS?. Pipe diameter 400mm thickness 8mm. Which code and reference need to be follow?. Thank you.
>
> Mohd Firdaus Abd Rahim
> QA/QC
> +60122796361
>
> Sent from my iPhone
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
> From: mohdfirdaus.abdrahim77@gmail.com
> Date: Mon, 21 Jul 2014 22:48:23 +0800
> To: materials-welding@googlegroups.com
>
> Dear all,
>
> Can anybody guide me for preparation HDPE WPS?. Pipe diameter 400mm thickness 8mm. Which code and reference need to be follow?. Thank you.
>
> Mohd Firdaus Abd Rahim
> QA/QC
> +60122796361
>
> Sent from my iPhone
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
Comments