POST-WELD TREATMENT of SS

To ensure satisfactory corrosion resistance for the welded joint, slag, spatter and oxides must be removed. Welding oxide is rich in chromium, which means that the material underneath the oxide has been depleted of chromium, thereby reducing its resistance to pitting corrosion. Post-weld treatment is therefore very important if the weld is to be exposed to acidic or neutral; chloride containing solutions such as seawater and pulp bleach plant liquids.

 

In these cases, pickling should be carried out to remove this oxide and enable the formation of a new protective and passivating oxide layer. Note that failure to use sufficient shielding gas during pipe welding may result in oxidation of the root side. In such cases the root side has to be cleaned by mechanical or chemical means.

 

Annealing

Stress-relief annealing of a non-stabilized stainless steel at temperatures within the range 550-650°C involves a risk of chromium carbide precipitation and might reduce the resistance to wet corrosion. Stabilized material however can undergo stress-relief annealing within the temperature range 550-650°C without any problems.

The safest method is to carry out stress-relief annealing at temperatures in excess of 1,000°C. The temperature levels can be provided by the manufacturer.

 

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...