Re: [MW:32911] ER309L DMW

ERNiCr3 and equivalent  On Wed, 23 Feb 2022, 09:29 fikril shaharudin, < ahmadfikrilkhairi@gmail.com > wrote: what should we use if the service temperature greater than 300 degree C? On Sat, Feb 19, 2022 at 10:51 PM pradip kumar Sil < pradipsil@gmail.com > wrote: you can use it if the service temp is not greater than 300-degree centigrade On Sat, Feb 19, 2022 at 7:51 PM pradip kumar Sil < pradipsil@gmail.com > wrote: Yes, you can On Sat, Feb 19, 2022 at 7:31 PM Tajuddin Mohammed < tajuddinjntu@gmail.com > wrote: Dear experts,       Please kindly clarify if we can use ER309L filler wire for dissimilar welding between P1(A106 Gr B) to P8 (A182 F316L) in gas service  Your valuable suggestion is highly appreciated. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and ...

[MW:32911] ASME 2021 implementation

Dear all, Can someone please tell me when asme 2021 editions implementation begins. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c2b33332-fae4-435d-87c1-a59e0b718a21n%40googlegroups.com .

Re: [MW:32911] shall we refer ASME sec VIII div-1 for soaking hours of normalising & tempering process-reg

Hi, For materials, we have to refer ASME Sec.II Part-A , SA217 and SA703 - S22. S22. Heat Treatment S22.1 Test specimens shall be heat treated together with the castings they represent. Heat-treated specimens shall be tested and shall meet the tensile and impact properties specified. S22.2 The remaining test specimens from Supplementary Requirement S22.1 representing the casting shall be treated thermally after the final (foundry) heat treatment to simulate heat treatments below the critical temperature that the casting may receive during fabrication, and then tested for mechanical properties. Time, temperature, and cooling rate shall be as stated in the order. In the case of postweld heat-treatment, the total time at temperature or temperatures for the test material shall be at least 80% of the total time at temperature or temperatures during actual postweld heat-treatment of the fabrication of which the casting or castings are a part. The total time at temperature or temperatures fo...

Re: [MW:32911] TOFD of SS welding

Dear sir , Why not possible by transverse waves ?? please clarify.. On Wed, Feb 23, 2022 at 9:29 AM George Dilintas < dilintas@gmail.com > wrote: with longitudinal waves only Στις Πέμ 17 Φεβ 2022 στις 5:22 π.μ., ο/η Manish Kumar < mkmkr431@gmail.com > έγραψε: Dear Sir, Please advise as per ASME or other Demonstration of SS welding for TOFD possible or not. Regards Manish Kumar -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k5ET5rTKnzG%2B-6c5h42Jo1BBVwhT5dEYR6fCHNkSL3Yug%40mail.gmail.com . -- Dr. Georgios Dilintas, Dipl. Ing. In Aeronautic and Space Engineering Ph.D in Mech...

Re: [MW:32906] P91 - Repair Welding and PWHT

and UW-38 in Section VIII-1 Στις Πέμ 17 Φεβ 2022 στις 5:22 π.μ., ο/η pradip kumar Sil < pradipsil@gmail.com > έγραψε: Hi Satish, ASME code is silent regarding this issue. Better go for client specification. Regards, Pradip On Wed, Feb 16, 2022 at 11:23 AM 'james gerald' via Materials & Welding < materials-welding@googlegroups.com > wrote: Please see a snap shot below from API 938B about Repair. Thanks & Regards J.Gerald Jayakumar On Tuesday, 15 February, 2022, 07:12:54 am GMT+4, Sathish V P < sathishvp86@gmail.com > wrote: Dear All, We have a scenario where the SA335P91 - Weld joint had 3 repairs and PWHT Cycles. Is there any code reference to limit the number of repairs / PWHT in the P91 weld joints or what permissible times PWHT could be done on the same joint. In this case - Pipe...

Re: [MW:32906] P91 - Repair Welding and PWHT

Check PW-40 in Section I of ASME,  Στις Πέμ 17 Φεβ 2022 στις 5:22 π.μ., ο/η pradip kumar Sil < pradipsil@gmail.com > έγραψε: Hi Satish, ASME code is silent regarding this issue. Better go for client specification. Regards, Pradip On Wed, Feb 16, 2022 at 11:23 AM 'james gerald' via Materials & Welding < materials-welding@googlegroups.com > wrote: Please see a snap shot below from API 938B about Repair. Thanks & Regards J.Gerald Jayakumar On Tuesday, 15 February, 2022, 07:12:54 am GMT+4, Sathish V P < sathishvp86@gmail.com > wrote: Dear All, We have a scenario where the SA335P91 - Weld joint had 3 repairs and PWHT Cycles. Is there any code reference to limit the number of repairs / PWHT in the P91 weld joints or what permissible times PWHT could be done on the same joint. In this case...

Re: [MW:32901] Feritic Steel

ferritic steels can be hardned  Στις Τετ 16 Φεβ 2022 στις 9:30 π.μ., ο/η Kannayeram Gnanapandithan < kgpandithan@gmail.com > έγραψε: Less Carbon, High Chrom and some small  addition of alloying elements Nb, Ni etc U can not hardened by heattreatment THANKS & BEST REGARDS, KG.PANDITHAN, BE, IWE,  CSWIP 3.1, ISO 9712 Level 2 in VT, ASNT-Level II in PT,MT,RT & UT, LA ISO 9001-2015, International Welding Engineer.  CONSULTANT-WELDING & QUALITY Mobile no: +919940739349 On Wed, Feb 16, 2022 at 8:52 AM SN < suryawanshinileshj@gmail.com > wrote: Dear all, What is the exact defination of ferritic steel as per ASME or ASTM or EN standard. Kindly clarify Regards  -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-w...