Re: [MW:35315] Low alloy steel Golden joint root NDT

You can select dry method dry powder MPO.

On Mon, 21 Oct, 2024, 9:48 am Karuppa Samy, <samyqc08@gmail.com> wrote:
Dear All,

How can we do root NDT for low alloy (HS service) steel golden, while doing continuous preheat ( 300°C) and can you recommend suitable NDT methods.

Regards
K. Karuppasamy,



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJg1Sz%3DuqTToO5iiTELw__bb6rQBueKDd_VPNcKTCFQNqqM8bw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CABYJxktXUO%3D2U_zj1_Y1GgPRFNfWkaV%2BwpwROJJF4P0zgRkH1g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...