Re: [MW:35314] P-No. of UNS 06626

P. no for UNS 06626 (inconel 625 LCF) is P45 and UNS 06625 (inconel 625) is P43.
Though both are Ni-Cr-Mo based, 06626 has more controlled microstructure for increased fatigue resistance 
at cyclic temperature conditions and is used for bellows and aerospace joints used at elevated temperatures. 
UNS n06625 is used for its high strength and corrosion resistance applications. 
Sridhar.

On Wed, 23 Oct 2024 at 15:29, saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear Team

   KINDLY SUGGEST PREHEAT TEMP. MIN. AND MAX. FOR INC625

 
Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936


On Mon, Mar 25, 2024 at 12:18 PM Vinay <vinay.thattey@gmail.com> wrote:
PL confirm , it is UNS N06626 . Its Ni-Cr moly steel..   P-45 is correct.
P-43 is for Inconel 625 i.e UNS 06625 . 

On Wed, 28 Feb 2024 at 15:42, ilham fauzi <ifilham@gmail.com> wrote:
Dear Experts,

What is P-No. of UNS 06626, my client say its P No.45 but that materials simillar with UNS 06625 which is its P-No.43. Please for the advice

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c105a43f-72c7-44b6-96e1-0e11095552a3n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29Oh4_KzW-XOuphs89C0sJ5YSoCX%3DEUdLaNiiuK3%2BxhoB-A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmsPa3KPgtthzTknbk_JUjcbfY0GvBGsA%3Dk3J9JgivYJQg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYiieijepV2TnD41ayiBubNtiXU6zoSVRR2VYG2UTK8eASg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...