Dear Team

   KINDLY SUGGEST PREHEAT TEMP. MIN. AND MAX. FOR INC625

 
Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936


On Mon, Mar 25, 2024 at 12:18 PM Vinay <vinay.thattey@gmail.com> wrote:
PL confirm , it is UNS N06626 . Its Ni-Cr moly steel..   P-45 is correct.
P-43 is for Inconel 625 i.e UNS 06625 . 

On Wed, 28 Feb 2024 at 15:42, ilham fauzi <ifilham@gmail.com> wrote:
Dear Experts,

What is P-No. of UNS 06626, my client say its P No.45 but that materials simillar with UNS 06625 which is its P-No.43. Please for the advice

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c105a43f-72c7-44b6-96e1-0e11095552a3n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29Oh4_KzW-XOuphs89C0sJ5YSoCX%3DEUdLaNiiuK3%2BxhoB-A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmsPa3KPgtthzTknbk_JUjcbfY0GvBGsA%3Dk3J9JgivYJQg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...