Thursday, November 7, 2024

[MW:35308] Tack weld requirements ASME / EN

Dears

regarding the tack weld I use the rod, both for supports installation EN 15609-1 and stainless steel piping installation according ASME IX.

There is any requirements that allow or prohibits to use the rod?

the rod with same material and certificate 3.1 etc etc.




Immagine 2024-10-17 145625.jpg


thank you 

Matteo 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/90bdad1a-997a-4edc-abeb-32b9e4c9da49n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS