Re: [MW:35293] SA335 P91 to SA106Gr.B Dissimilar Material Welding Procedure

P91 - P22 - TYP B91 /B3
P22 -P11- TYP B3/B2
P11-SA 106 - B2/ Carbon steel 

Normally Higher alloy of the consumables
Deployed 

You can decided based on PQR 
Vishwas-IWE
9823472273
Sent from my iPhone

On 23 Sep 2024, at 4:07 PM, Md Usman Ghani <mdushmanghani@gmail.com> wrote:



Which fillers have to use for P91-P22, nd P22-P11 , P11-106


On Sun, 22 Sept, 2024, 6:43 pm Vinay, <vinay.thattey@gmail.com> wrote:
Dear Friend :
Its not  a recommended combination. But can you please  describe its application? 

On Mon, 16 Sept 2024 at 13:07, Vijay Kumar <vijaytuty@gmail.com> wrote:
Dear Experts,

I need SA335 P91 to SA106Gr.B Dissimilar Material Welding Procedure with some reference codes. 

Please share 

Thanks 
Vijayakumar
+91 8238450968

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/be7e26e6-2446-4b69-8ed4-d10c5a074dcfn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29Oi9vFA7rrr1jFKxRXTkgVHex3_SofLnZf0qaPCQ5M7LaA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP4SqnXEMYaC_aPg6V75kth%2BuG0YO3N1Q_Ef0LCJ%2BzAGX0-vQw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...