Thursday, June 27, 2024

Re: [MW:35083] WPS concern

Dear Nilesh,

No, you cannot use the same WPS for IS 2062 E250 material if it was qualified for IS 2062 E350 material. According to AWS D1.1, WPS qualifications are specific to the tensile strength of the material, and IS 2062 E250 and IS 2062 E350 have different tensile strengths (410 MPa vs. 490 MPa). A new WPS qualification is required for IS 2062 E250.  

Regards,

AB

On Sat, 22 Jun 2024 at 09:36, 'Quality SSFab' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hi,

We have qualified WPS as per AWS D1.1 for material IS 2062 E350 material , now we want to weld material IS2062 E250 material, Can we use the same WPS ?

as IS 2062 E250 - Tensile strength - 410 MPA & 
IS2062 E350 - Tensile strength - 490 MPA

Please suggest your views.. Urgent.



Regards,
SHRI SAMARTH FABRICATION LLP
NILESH R. GAVHANE
Quality Engineer
Mobile No.: 9970571796

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALReYKHfbWzPjfqXvLfruD8VKCvf80aLjZaNA5BywGmxU3SDOQ%40mail.gmail.com.


--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAADcG1oiaj20WGSKwa2B4%3D9zLXNuA0_9c5GGhyQhp4R%3DHLKXxA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...