IS 2062 is unassigned material as per
AWS D1.1

You will be using E7018 for both  IS2962 Gr 250 and IS 2062 Gr 350 

Speak to QAC and elaborate above details  that both are Carbon steels.
Unassigned to Unassigned is qualified and it qualifies 
Unassigned to Unassigned 
Grade is different but E 7018 mechanical  properties are compatible to both materials.

So is acceptable 
Sent from my iPhone

On 22 Jun 2024, at 9:36 AM, 'Quality SSFab' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Hi,

We have qualified WPS as per AWS D1.1 for material IS 2062 E350 material , now we want to weld material IS2062 E250 material, Can we use the same WPS ?

as IS 2062 E250 - Tensile strength - 410 MPA & 
IS2062 E350 - Tensile strength - 490 MPA

Please suggest your views.. Urgent.



Regards,
SHRI SAMARTH FABRICATION LLP
NILESH R. GAVHANE
Quality Engineer
Mobile No.: 9970571796

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALReYKHfbWzPjfqXvLfruD8VKCvf80aLjZaNA5BywGmxU3SDOQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...