Re: [MW:35062] SS clading on CS

Dear, 

Use 309Mo for better results 

On Wed, Jun 5, 2024 at 1:21 PM Mashood Khan <mashood@epic.com.pk> wrote:
Dear, 
The current circumstances is ,
Vessel is SS316 and I am welding a SS316 4mm plate on the CS flange as a cladding.
I want to know if I weld the SS316 Cladding plate on CS Flange with SS309. is it any problem with their composition?
Second is that SS309 is compatible with SS316 if I totally weld with SS309 Electrode.

Regards,
Mailsuite Sent with Mailsuite  ·  Unsubscribe
06/05/24, 12:42:33 PM

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD3cn5hS2LbPHDo%3DciN_dsPUK9X-97b33KRO80PYso_cLw6rjw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGAT7zeJZ%3DnUqsNudmM55vMaQyVuvck1DsmDG43-FMmy9r1OhQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...