Re: [MW:35048] Difference of 2% of Chromium Content on the Actual PMI VS Sec IIA

It's is acceptable 

On Fri, 31 May 2024, 10:11 pradip kumar Sil, <pradipsil@gmail.com> wrote:
You can refer PFI  ( Pipe fabrication Institute ) or 10 % bi lateral tolerance of actual alloy content from code for the base metal.

On Fri, May 17, 2024 at 12:14 PM Dinesh Baskaran <dinesh09nov@gmail.com> wrote:

Plz refer attach 

Thank and regards

Dinesh Baskaran


On Thu, 16 May, 2024, 12:05 pm Macario Jr. Palola, <macario.palola@gmec.ph> wrote:
Sirs,

May I ask your valuable inputs with regards to my queries.
Base on the attached report, the actual value of %Cr is 20% as per PMI and the value of %Cr in ASME Sec IIA. Now my question, is this acceptable or not ?

Thank you in advance.

Regards,

Mac

The information contained in this email is intended for use only by the recipient to whom or which this is addressed. Such information may be privileged, confidential, and/or proprietary subject to the GMEC Email Disclaimer. Moreover, as we value your privacy, we will handle and safeguard any personal data we receive in this email in accordance with our Privacy Notice.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a98f67f1-0f70-4e02-ac62-785bd8abddf1n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMAJDVoHNBxpdntmSf%2B%3DYPP0LZ4sEZLUsw6dY_46eDr4xdU43w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8nXoiE-wYcMf_9Cj9MArocd11vsmdLy-MwSK3CoMON5yQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGr8UaZ-GJnYGbrQjozc1kHTyutwTvuOJSUxCuqzKLmHGaO%3DrQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...