Re: [MW:34738] Re: Welding 2 different pipe grades together depending on API 1104

You stated two available WPS without stating the material you intent to weld. It is not possible to advise you on applicable wps without knowledge of the material to be welded.

On Wednesday, 10 January 2024 at 09:04:34 GMT+1, Pipeline Welding <prakashbontra@gmail.com> wrote:



SAES-W-12
7.4.1 Procedures for API SPEC 5L Grade X65 or higher shall be qualified for each specific material grade, where each grade includes the equivalent flanges and fittings with same SMYS and similar CEq. Qualification on API SPEC 5L grade X65 shall also qualify all lower grades 0 (including Grade B) for both API STD 1104 and ASME SEC IX.
On Tuesday, January 9, 2024 at 3:03:02 PM UTC+3 dia shukr wrote:
Hi friends

I have an existing pipeline with qualified WPS#1(API 5L Grade X60 Thick. 12.7mm) and a new pipeline with qualified WPS#2(API 5L Grade X65 Thick.17.48mm).
My question is do I need a new qualification WPS or I can follow WPS#2??

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/d39776f5-3ba0-4f2c-be32-93d8b6a464d4n%40googlegroups.com
.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...